Dual-Additive Si-Graphite
Online Inquiry

Dual-Additive Si-Graphite

Dual-Additive Si-Graphite

Cat No:BME-0048

Description

Optimized for silicon-graphite blended anodes (5-15% Si), balancing high FEC for Si stability and VC for graphite protection.

Basic Information

Main Salt LiPF6
Salt Concentration 1.1 M
Solvent Ratio (Vol%) EC:EMC:DEC=1:7:2
Additive 1 FEC (10%)
Additive 2 VC (2%)
Appearance Colorless Liquid
Water Content (KF) ≤ 15 ppm
Free Acid (as HF) ≤ 30 ppm
Density (25°C) 1.24-1.34 g/cm³
Conductivity (25°C) 8.5-10.5 mS/cm
Viscosity (25°C) 3.5-5.0 mPa·s
Chloride (Cl-) ≤ 1 ppm
Sulfate (SO4 2-) ≤ 5 ppm
Iron (Fe) Content ≤ 1 ppm
Sodium (Na) Content ≤ 2 ppm
Potassium (K) Content ≤ 2 ppm
Operating Voltage 0.0 - 4.35 V
Operating Temp -20 to 55°C
Flash Point 28-38°C
Solid Content 14-17 wt%
Refractive Index 1.36-1.44
Turbidity ≤ 5 NTU
Color (APHA) ≤ 30
Packaging SS Cylinder
Storage < 5°C, Ar

GET IT!

Eata Battery is the single source for every high-performance material in next-gen batteries—from cathode powders to current collectors, catalysts to membranes. We de-risk your supply chain so you can scale faster.

Contact Us

For Research or Industrial Raw Materials, Not For Personal Medical Use!

0
0

There is no product in your cart.