This high-purity ferrous oxalate dihydrate (FeC2O4.2H2O) powder from Eata Battery serves as one of the essential metal-precursor raw materials for synthesizing lithium iron phosphate (LiFePO4, LFP) cathode powder, particularly in solid-state carbothermal reduction and oxalate co-precipitation production routes. It is a pale yellow crystalline powder with a relative density of 2.28 that decomposes at 160 degrees C; it is soluble in acids and practically insoluble in water, so it stays uniformly distributed through the dry-blended precursor mixture until thermal decomposition begins. Specifications: purity > 99%; hydrochloric acid insolubles <= 0.005%; chloride <= 0.002%; sulfate <= 0.05%; ammonium <= 0.05%; alkaline earth metals <= 0.1%. These tight impurity limits minimize chloride corrosion of furnace equipment, sulfate poisoning of the carbon-coating catalyst, and alkali-earth substitution in the olivine lattice. Supplied as a free-flowing powder in 500 g bottles for laboratory and pilot-scale LFP production.
| Chemical Formula | FeC2O4.2H2O |
| Molecular Weight | 179.9 |
| Storage Conditions | Store at room temperature, dry and sealed |
| Purity | >99% |
| Primary Application | Iron precursor for LFP (LiFePO4) cathode synthesis via carbothermal reduction and oxalate co-precipitation routes |
| English Synonyms | iron(II) oxalate dihydrate; iron oxalate |
| Density | 2.28 |
| Solubility | Soluble in acids; practically insoluble in water |
| Melting Point | 160 °C (decomposes) |
| Shipping Conditions | Ships at ambient temperature |
| Available Package Sizes | 500 g |
Eata Battery is the single source for every high-performance material in next-gen batteries—from cathode powders to current collectors, catalysts to membranes. We de-risk your supply chain so you can scale faster.
For Research or Industrial Raw Materials, Not For Personal Medical Use!
|
There is no product in your cart. |