Low-Temperature Electrolyte
Online Inquiry

Low-Temperature Electrolyte

Low-Temperature Electrolyte

Cat No:BME-0003

Description

Optimized for extreme environments, using low-viscosity solvents to maintain ion mobility and capacity at sub-zero temperatures.

Basic Information

Main Salt LiPF6
Salt Concentration 1.0 M
Solvent Ratio (Vol%) EC:EMC:DEC=1:1:8
Additive 1 FEC (2%)
Additive 2 VC (1%)
Appearance Colorless Liquid
Water Content (KF) ≤ 20 ppm
Free Acid (as HF) ≤ 50 ppm
Density (25°C) 1.15-1.25 g/cm³
Conductivity (25°C) 6.5-8.5 mS/cm
Viscosity (25°C) 2.5-4.5 mPa·s
Chloride (Cl-) ≤ 1 ppm
Sulfate (SO4 2-) ≤ 5 ppm
Iron (Fe) Content ≤ 1 ppm
Sodium (Na) Content ≤ 2 ppm
Potassium (K) Content ≤ 2 ppm
Operating Voltage 0.0 - 4.2 V
Operating Temp -40 to 45°C
Flash Point 20-30°C
Solid Content 11-13 wt%
Refractive Index 1.34-1.44
Turbidity ≤ 5 NTU
Color (APHA) ≤ 30
Packaging SS Cylinder
Storage < 5°C, Ar

GET IT!

Eata Battery is the single source for every high-performance material in next-gen batteries—from cathode powders to current collectors, catalysts to membranes. We de-risk your supply chain so you can scale faster.

Contact Us

For Research or Industrial Raw Materials, Not For Personal Medical Use!

0
0

There is no product in your cart.