Scandia-Stabilized Zirconia Substrate (ScSZ-10)
Online Inquiry

Scandia-Stabilized Zirconia Substrate (ScSZ-10)

Scandia-Stabilized Zirconia Substrate (ScSZ-10)

Cat No:FCEM-0009

Description

A high-conductivity ceramic electrolyte substrate for intermediate temperature SOFCs, offering nearly double the ionic conductivity of traditional YSZ.

Basic Information

Polymer/Material Base 10 mol% Sc2O3-ZrO2
Ion Exchange Capacity (IEC) N/A
Ionic Conductivity (S/cm) 0.15 - 0.25 (at 800°C)
Thickness (μm) 150 - 200
Tensile Strength (MPa) 300 - 400
Elongation at Break (%) < 0.1
Max Operating Temp (°C) 1000
Chemical Stability (Fenton’s Test) Excellent
Density (g/cm³) 5.75
Ash Content (%) < 0.01
EW (Equivalent Weight) N/A
Glass Transition Temp (Tg) N/A
Storage Humidity (%) 0 - 95
Storage Temp (°C) Any
Solubility in Polar Solvents Insoluble
Ionic Resistance (Ω·cm²) 0.1
Dimensional Stability (%) < 1
Thermal Stability (TGA) > 1800°C
Flammability Rating Non-flammable
Surface Roughness (Ra) < 0.3 μm

GET IT!

Eata Battery is the single source for every high-performance material in next-gen batteries—from cathode powders to current collectors, catalysts to membranes. We de-risk your supply chain so you can scale faster.

Contact Us

For Research or Industrial Raw Materials, Not For Personal Medical Use!

0
0

There is no product in your cart.